Sign In | Join Free | My polstate.com |
|
Brand Name : YUHONG
Model Number : UNS: S31035, 1.4990, X7NiCrWCuCoNb25-23-3-3-2
Certification : ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008
Place of Origin : China
MOQ : 100KGS
Price : negotiable
Payment Terms : T/T, L/C
Supply Ability : 1500 tons per month
Delivery Time : 10days->
Packaging Details : Ply-wooden Case /Iron Case/ Bundle with plastic Cap
Standard : EN10216-5 , DIN 17456, DIN 17458, ASTM A213, ASME SA213, JIS G3459, G3463 , GOST 9941
Material : UNS: S31035, 1.4990, X7NiCrWCuCoNb25-23-3-3-2
Size-OD : 73MM
Size-Thickness : 20BWG, 18BWG, 16BWG, 14BWG, 12BWG, 10BWG, 8BWG
Length : 6000mm to 8000mm
NDT : ET, UT, HT,
Application : coal fired steam boilers
ASME SA213 Sanicro 25 22Cr25NiWCoCu Austenitic Stainless Steel for Steam Boilers
Yuhong Group's Sanicro 25 is an austenitic 22Cr25NiWCoCu stainless steel material with excellent high-temperature properties designed for use in advanced pulverised coal steam boilers.
The new heat-resistant steel, SA-213 S31035 (22Cr25Ni3W3CuCoNbN), is currently recognized as one of the main candidate materials for power plants due to its exceptional strength.
The results of the creep tests demonstrated that S31035 steel exhibits significantly higher creep strength compared to S30432 steel, with an extrapolated creep rupture strength of approximately 118.0 MPa after 50,000 hours at 700°C. Additionally, it displayed excellent fracture toughness, with a fracture surface contraction exceeding 50%. The exceptional creep strength of S31035 steel is attributed to the combined precipitation strengthening of nanoscale Cu-rich phases, acicular Laves phases, and secondary Z phases.
C | Si | Mn | P | S | Cr | Ni | W | Co | Cu | Nb | N |
---|---|---|---|---|---|---|---|---|---|---|---|
≤0.1 | 0.2 | 0.5 | ≤0.025 | ≤0.015 | 22.5 | 25 | 3.6 | 1.5 | 3.0 | 0.5 | 0.23 |
Sanicro 25 Solution annealing
1180-1250°C (2155-2280°F) and quenched.
Sanicro 25 Physical properties
Density: 8.32 kg/dm3; 0.29 lb/in3
Temperature, oC | W/(m oC) | Temperature, oF | Btu/(ft h oF) |
---|---|---|---|
20 | 12 | 68 | 7 |
100 | 13 | 100 | 7 |
200 | 15 | 200 | 7.5 |
300 | 16 | 400 | 9 |
400 | 18 | 600 | 10 |
500 | 20 | 800 | 11 |
600 | 22 | 1000 | 12 |
700 | 23 | 1200 | 13 |
800 | 25 | 1400 | 14.5 |
900 | 27 | 1600 | 15.5 |
1000 | 28 | 1800 | 16.5 |
1100 | 30 | 2000 | 17.5 |
Temperature, oC | J/(kg oC) | Temperature, oF | Btu/(lb oF) |
---|---|---|---|
20 | 470 | 68 | 0.11 |
100 | 485 | 100 | 0.11 |
200 | 500 | 200 | 0.12 |
300 | 520 | 400 | 0.12 |
400 | 535 | 600 | 0.12 |
500 | 555 | 800 | 0.13 |
600 | 570 | 1000 | 0.13 |
700 | 585 | 1200 | 0.14 |
800 | 605 | 1400 | 0.14 |
900 | 620 | 1600 | 0.15 |
1000 | 640 | 1800 | 0.15 |
1100 | 665 | 2000 | 0.16 |
Sanicro 25 Mean values
Temperature, oC | µΩm | Temperature, oF | µΩin. |
---|---|---|---|
20 | 0.98 | 68 | 38.6 |
Temperature, oC | Per oC | Temperature, oF | Per oF |
---|---|---|---|
30-100 | 14.5 | 86-200 | 8 |
30-200 | 1.5. | 86-400 | 8.5 |
30-300 | 16 | 86-600 | 8.5 |
30-400 | 16 | 86-800 | 9 |
30-500 | 16.5 | 86-1000 | 9 |
30-600 | 16.5 | 86-1200 | 9.5 |
30-700 | 17 | 86-1400 | 9.5 |
30-800 | 17 | 86-1600 | 9.5 |
30-900 | 17.5 | 86-1800 | 10 |
30-1000 | 18 | 86-2000 | 10 |
30-1100 | 18.5 |
![]() |